5A06合金TIG焊接头敏化失效机制及还原调控 |
| 李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏 |
|
Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy |
| LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin |
| 图7 5A06合金焊接态、敏化及还原样品不同区域的硝酸失重法(NAMLT)测试结果 |
| Fig.7 NAMLT results of different regions in as-welded, sensitized, and reversion treated 5A06 alloy samples |
|