5A06合金TIG焊接头敏化失效机制及还原调控
李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏

Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy
LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin
图6 5A06合金焊接态、敏化及短时还原样品经56%H3PO4溶液腐蚀后不同区域显微组织的SEM像
Fig.6 SEM images of as-welded (a, d, g); 175 oC, 100 h sensitized (b, e, h); and 310 oC, 1 h short-term reversion treated (c, f, i) 5A06 alloy samples after immersion in 56%H3PO4 (Insets in Figs.6a and h show the enlarged images of rectangular areas. Arrows in the inset of Fig.6a indicate corrosion pits discontinuously distributed along the grain boundary) (a-c) BM (d-f) HAZ (g-i) WZ