5A06合金TIG焊接头敏化失效机制及还原调控 |
| 李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏 |
|
Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy |
| LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin |
| 图2 5A06合金焊接态样品显微组织的OM像和母材(BM)、热影响区(HAZ)、焊缝区(WZ)的EBSD反极图 |
| Fig.2 OM image of as-welded 5A06 alloy sample (a) and EBSD inverse pole figures of BM (b), HAZ (c), and WZ (d) (d—average grain size) |
|