5A06合金TIG焊接头敏化失效机制及还原调控 |
| 李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏 |
|
Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy |
| LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin |
| 图1 5A06合金焊接板材显微组织观察及腐蚀实验样品取样示意图 |
| Fig.1 Schematics of locations of microstructure observation and corrosion test samples within 5A06 alloy welded plates (L—welding direction and rolling direction, T—transverse direction, S—thickness direction. BM—base metal, HAZ—heat-affected zone, WZ—weld zone, NAMLT—nitric acid mass loss test, sp.—specimen) |
|