直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制
王明飞, 陶美悦, 宫臣, 彭博, 李廷举, 接金川

Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing
WANG Mingfei, TAO Meiyue, GONG Chen, PENG Bo, LI Tingju, JIE Jinchuan
图11 S1~S4样品Cu-Ni-Si合金侧和1010钢侧的局部取向差(KAM)图及对应的几何必需位错密度分布统计图
Fig.11 Dislocation analyses of samples S1-S4 (a1-d1) kernel average misorientation (KAM) maps of Cu-Ni-Si alloy side in samples S1 (a1), S2 (b1), S3 (c1), and S4 (d1) (a2-d2) geometrically necessary dislocation (GND) density distributions corresponding to Figs.11a1-d1, respectively (GNDave.—average GND density) (a3-d3) KAM maps of 1010 steel side in samples S1 (a3), S2 (b3), S3 (c3), and S4 (d3) (a4-d4) GND density distributions corresponding to Figs.11a3-d3, respectively