直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制 |
| 王明飞, 陶美悦, 宫臣, 彭博, 李廷举, 接金川 |
|
Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing |
| WANG Mingfei, TAO Meiyue, GONG Chen, PENG Bo, LI Tingju, JIE Jinchuan |
| 图7 S1~S4样品从Cu-Ni-Si侧到1010钢侧的硬度分布曲线和平均硬度 |
| Fig.7 Microhardness distribution curves (a) and average microhardnesses (b) of samples S1-S4 in Cu-Ni-Si side, 1010 steel side, and interface (The negative values of position in Fig.7a indicate the Cu-Ni-Si side, positive values indicate the 1010 steel side, and the coordinate origin “0.0” is defined as the center of the interface, respectively) |
|