直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制
王明飞, 陶美悦, 宫臣, 彭博, 李廷举, 接金川

Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing
WANG Mingfei, TAO Meiyue, GONG Chen, PENG Bo, LI Tingju, JIE Jinchuan
图6 S1~S3样品中Cu-Ni-Si基体和析出相的TEM表征
Fig.6 TEM characterizations of Cu-Ni-Si matrix and precipitation phases in samples S1 (a-c), S2 (d-f), and S3 (g-i) (a, d, g) bright field TEM images of Cu-Ni-Si matrix (b, e, h) HRTEM images of square areas in Figs.6a, d, and g, respectively (Insets in Figs.6b and e show the corresponding SAED patterns) (c, f) bright field TEM images of precipitation phases at grain boundary (Insets show the corresponding SAED patterns) (i) TEM image and corresponding EDS element distribution maps of sample S3