直接退火与冷轧+退火处理Cu-Ni-Si/1010钢双金属复合材料的组织演变及强化机制 |
| 王明飞, 陶美悦, 宫臣, 彭博, 李廷举, 接金川 |
|
Microstructural Evolution and Strengthening Mechanisms of Cu-Ni-Si/1010 Steel Bimetallic Composites via Direct Annealing and Cold Rolling + Annealing |
| WANG Mingfei, TAO Meiyue, GONG Chen, PENG Bo, LI Tingju, JIE Jinchuan |
| 图3 S1~S4样品界面处的EPMA线扫描结果 |
| Fig.3 EPMA line scan results at the interfaces of samples S1 (a), S2 (b), S3 (c), and S4 (d) |
|