TC4钛合金循环变形微观组织演化与滑移机制
吴帆, 刘华辉, 边文珊, 蔡竣宇, 金士杰, 罗忠兵

Microstructural Evolution and Slip Mechanisms in TC4 Titanium Alloy During Cyclic Deformation
WU Fan, LIU Huahui, BIAN Wenshan, CAI Junyu, JIN Shijie, LUO Zhongbing
图8 不同循环周次下循环变形TC4合金滑移系的Schmid因子演变
Fig.8 Schmid factor evolutions of slip systems in cyclically deformed TC4 alloy (AVG—average of schmid factor)
(a) basal <a> slip (b) prismatic <a> slip (c) pyramidal <a> slip
(d) pyramidal 1st <c + a> slip (e) pyramidal 2nd <c + a> slip