TC4钛合金循环变形微观组织演化与滑移机制 |
| 吴帆, 刘华辉, 边文珊, 蔡竣宇, 金士杰, 罗忠兵 |
|
Microstructural Evolution and Slip Mechanisms in TC4 Titanium Alloy During Cyclic Deformation |
| WU Fan, LIU Huahui, BIAN Wenshan, CAI Junyu, JIN Shijie, LUO Zhongbing |
| 图3 TC4合金循环加载响应:应力-应变滞后环及塑性应变幅与循环加载周次曲线 |
| Fig.3 Cyclic loading response of TC4 alloy (a) stress-strain hysteresis loops (N—loading cycle) (b) plastic strain amplitude ( |
|