Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
表4 图15中点1~6的EDS成分分析结果
Table 4 Chemical compositions of the spots 1-6 in Fig.15 determined by EDS
SpotAtomic fraction / %Possible phase
OAlSiMo
126.087.5666.36-SiO2, Al2O3
23.98-34.0961.93Mo5Si3
32.20-64.8033.00MoSi2
457.585.8134.761.85SiO2, Al2O3
55.92-34.5259.56Mo5Si3
62.25-64.7433.01MoSi2