Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
表3 图14中点1~6点的EDS成分分析结果
Table 3 Chemical compositions of the spots 1-6 in Fig.14 determined by EDS
SpotAtomic fraction / %Possible
BOSiMophase
1-4.5034.5960.91Mo5Si3
2-4.9034.3260.78Mo5Si3
3--35.7364.27Mo5Si3
4--34.4365.57Mo5Si3
550.11-0.2949.60MoB
638.27-0.3161.42Mo2B