Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
表2 图13中点1~9的EDS成分分析结果
Table 2 Chemical compositions of the spots 1-9 in Fig.13 determined by EDS
SpotAtomic fraction / %Possible phase
OAlSiMo
13.12-62.7334.15MoSi2
267.720.6030.770.91SiO2
354.685.7339.59-SiO2, Al2O3
43.42-63.1333.45MoSi2
547.439.6033.249.73SiO2, Al2O3, MO3
655.486.1736.851.50SiO2, Al2O3
750.6013.6220.5215.26SiO2, Al2O3, MO3
843.3910.7735.6610.18SiO2, Al2O3, MO3
954.9610.1434.90-SiO2, Al2O3