Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
表1 图3中点1~8的EDS成分分析结果
Table 1 Chemical compositions of the spots 1-8 in Fig.3 determined by EDS
CoatingLayerSpotAtomic fraction / %Possible phase
BSiMo
Silicide coatingLayer I1-65.8034.20MoSi2
Layer II2-37.6462.36Mo5Si3
Silicide-boride composite coatingLayer I3-64.2135.79MoSi2
Layer II451.440.5548.01MoB
5-67.0532.95MoSi2
Layer III60.7636.3862.86Mo5Si3
Layer IV759.25-40.75MoB
Layer V830.95-69.05Mo2B