Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
图11 硅化物涂层及硅化物-硼化物复合涂层在1200 ℃的氧化动力学曲线
Fig.11 Oxidation kinetics curves of silicide coating and silicide-boride composite coating at 1200 oC