Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
图7 不同保温时间下硅化物-硼化物复合涂层截面形貌的SEM像
Fig.7 Cross-sectional SEM images of silicide-boride composite coating at holding time of 0 h (a-c), 1.5 h (d), 3 h (e), and 10 h (f) (Inset in Fig.7a shows the locally enlarged image of the rectangle zone)