Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为
吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞

Microstructure and High-Temperature Oxidation Behavior of Silicide-Boride Composite Coatings on the Surface of Mo
WU Zhou, WU Fan, WANG Yiming, GAN Youliang, FU Xuesong, CHEN Guoqing, ZHOU Wenlong, ZU Yufei
图2 硅化物涂层和硅化物-硼化物复合涂层表面形貌的SEM像和EDS分析
Fig.2 Surface SEM images of the silicide coating (a) and silicide-boride composite coating (b) (Insets in Figs.2a and b show the corresponding grain size distributions); EDS analyses of spot 1 (c) and spot 2 (d) in Fig.2b