950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为
邓尕平, 赵杰, 高凯, 王威, 刘欢, 曹铁山, 程从前

Hot Corrosion Behavior of DZ411 Nickel-Based Superalloy NiCoCrAlY Coating at 950 oC
DENG Gaping, ZHAO Jie, GAO Kai, WANG Wei, LIU Huan, CAO Tieshan, CHENG Congqian
图9 DZ411合金NiCoCrAlY涂层中可能形成腐蚀产物的Gibbs自由能
Fig.9 Gibbs free energies (ΔG) of possible corrosion products forming in DZ411 alloy and NiCoCrAlY coating
(a) oxides (b) sulfides (c) chlorides/nitrides