950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为 |
| 邓尕平, 赵杰, 高凯, 王威, 刘欢, 曹铁山, 程从前 |
|
Hot Corrosion Behavior of DZ411 Nickel-Based Superalloy NiCoCrAlY Coating at 950 oC |
| DENG Gaping, ZHAO Jie, GAO Kai, WANG Wei, LIU Huan, CAO Tieshan, CHENG Congqian |
| 图8 各腐蚀层厚度和硫化物扩散深度统计 |
| Fig.8 Statistics of corrosion layer thicknesses and sulfide diffusion depth |
|