950 ℃下DZ411镍基高温合金NiCoCrAlY涂层热腐蚀行为 |
| 邓尕平, 赵杰, 高凯, 王威, 刘欢, 曹铁山, 程从前 |
|
Hot Corrosion Behavior of DZ411 Nickel-Based Superalloy NiCoCrAlY Coating at 950 oC |
| DENG Gaping, ZHAO Jie, GAO Kai, WANG Wei, LIU Huan, CAO Tieshan, CHENG Congqian |
| 图7 热腐蚀200 h后纯硫盐和混合盐试样截面的EDS线扫描结果 |
| Fig.7 EDS line scanning results of cross-section of specimens after 200 h hot corrosion under different salt film conditions (Insets are cross-sectional BSE images) (a) Na2SO4 salt film (b) Na2SO4 + NaCl salt film |
|