热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响 |
| 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏 |
|
Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy |
| WANG Bin, ZHAO Peng, LIU Jiawei, ZHANG Chunbo, QIN Zhiwei, DONG Honggang, LI Peng |
| 图11 1080 ℃ SA接头平均晶粒尺寸分布 |
| Fig.11 Average grain size distributions of different regions in 1080 oC SA joint |
|