热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响 |
| 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏 |
|
Effect of Heat Treatment on Microstructural Evolution and Mechanical Properties of Inertial Friction Welded Joints for FGH96 Superalloy |
| WANG Bin, ZHAO Peng, LIU Jiawei, ZHANG Chunbo, QIN Zhiwei, DONG Honggang, LI Peng |
| 图6 焊态及不同焊后热处理态接头焊核区(WZ)和母材(BM)区强化相分布的SEM像 |
| Fig.6 SEM images showing strengthening phase distributions in WZ (a1-e1) and BM zones (a2-e2) of welded joint (a1, a2) and post-weld heat treatment joints under different conditions (b1-e1, b2-e2) (a1, a2) AS (b1, b2) DA (c1, c2) 1030 oC SA (d1, d2) 1080 oC SA (e1, e2) 1140 oC SA |
|