表1 GH4065A和IN718高温合金的化学成分 (mass fraction / %)
Table 1 Chemical compositions of GH4065A and IN718 superalloys
AlloyCCrCoWMoAlTiNbZrBFeNi
GH4065A0.01116.0013.04.04.002.103.700.700.050.0151.00Bal.
IN7180.01019.39--3.050.531.025.21--16.69Bal.