热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响 |
| 秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚 |
|
Effect of Heat Treatment on Interfacial Microstructure of Inertial Friction Welded Joints for GH4065A/IN718 Dissimilar Superalloys |
| QIN Zhiwei, WANG Bin, ZHAO Qiang, LI Jiachen, SUN Yutao, HONG Xiaolong, LI Peng, DONG Honggang |
| 图1 焊态和热处理态接头沿轴向各区域显微组织的OM像 |
| Fig.1 Low (a, e) and high (b-d, f-h) magnified OM images of welded joint (a-d) and post-weld heat treated joint (e-h) (The black and yellow arrows in Figs.1a and e denote the widths of the weld zone (WZ) and thermo-mechanically affected zone (TMAZ) on IN718 side, respectively) (b, f) WZ (c, g) TMAZ on GH4065A side (d, h) TMAZ on IN718 side |
|