AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化
许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平

Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy
XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping
表4 热机械处理后Al1Cr1合金不同温度下各相的晶格常数和体积分数
Table 4 Lattice parameters and volume fractions of each phase at different temperatures for Al1Cr1 alloy after thermomechanical processing
Temperature oCaγ nmaα nmfγ %fα %
400.3592570.28676592.02057.9795
500.3592780.28678692.12547.8746
600.3592950.28678892.12717.8729
700.3593020.28680292.21187.7882
800.3593140.28680792.31907.6810
900.3593350.28681092.41097.5891
1000.3593460.28682092.49927.5008