许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平

Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy
XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping
表3 图3b中衍射峰强度的理论值和不同温度下的测量值
Table 3 Theoretical and measured intensities of diffraction peaks in Fig.3b
Item

fcc

(111)

bcc

(110)

fcc

(200)

bcc

(200)

fcc

(220)

bcc

(211)

fcc

(311)

fcc

(222)

Rhkl100.0100.042.250.017.680.06.54.5
40 oC13523.02784.002114.34497.251147.74424.121189.31544.36
50 oC13501.09769.092104.07447.971117.16441.421092.35524.49
60 oC13318.11754.632138.23489.521147.14434.471270.59530.41
70 oC13408.39754.182162.88478.251180.26431.021263.75516.45
80 oC13627.21755.642149.57477.471151.49405.401178.39539.94
90 oC13394.20758.282137.34435.911110.13425.501136.75549.34
100 oC13571.93749.342143.34443.711104.66396.191149.75535.87