AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化 |
||||||||||||||||
| 许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平 | ||||||||||||||||
|
Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy |
||||||||||||||||
| XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping | ||||||||||||||||
| 表2 均匀化热处理后低膨胀合金的拉伸强度和塑性 |
||||||||||||||||
| Table 2 Tensile strengths and ductilities of the low-expansion alloys after homogenization |
||||||||||||||||
|
||||||||||||||||