AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化
许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平

Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy
XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping
图5 热机械处理后Al1Cr1合金的微观组织表征
Fig.5 Microstructure characteristics of the Al1Cr1 alloy after thermomechanical processing
(a) BSE image (b) synchrotron XRD pattern
(c) EBSD IPF (d) EBSD phase distribution map