AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化
许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平

Composition Design and Optimization of Microstructure and Properties for an AlCrFeCoNi Low-Expansion Alloy
XU Dingfeng, HAN Feiyang, JIANG Qicheng, WANG Huan, SHANG Liyuan, LU Yiping
图3 Al1Cr1合金的物相分析
Fig.3 Phase analyses of the Al1Cr1 alloy
(a) calculated phase diagram (b) synchrotron XRD pattern
(c) EBSD inverse pole figure (IPF) (d) EBSD phase distribution map