高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响
王玮, 张宇博, 赵燕, 王同敏, 李廷举

Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment
WANG Wei, ZHANG Yubo, ZHAO Yan, WANG Tongmin, LI Tingju
图7 Al12Si-HEA试样中Si相的数量密度和平均直径随固溶时间的变化曲线
Fig.7 Variation curves of number densities and average diameters of Si phase in Al12Si-0%HEA and Al12Si-3%HEA samples with solution treatment time (t)