高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响
王玮, 张宇博, 赵燕, 王同敏, 李廷举

Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment
WANG Wei, ZHANG Yubo, ZHAO Yan, WANG Tongmin, LI Tingju
图6 固溶不同时间后Al12Si-3%HEA试样的TEM分析
Fig.6 TEM analyses of Al12Si-3%HEA samples with 0 h (a-d) and 1 h (e, f) solution treatments (a, e) TEM images of samples (b, f) corresponding EDX elemental maps of selected regions in Fig.4a (b) and Fig.4e (f) (c, d) HRTEM images and SAED patterns (insets) of cell boundary (d—interplanar spacing)