高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响
王玮, 张宇博, 赵燕, 王同敏, 李廷举

Influences of High-Entropy Alloy Particles on the Microstructure and Mechanical Properties of Selective Laser Melted Al12Si Alloy During Solution Treatment
WANG Wei, ZHANG Yubo, ZHAO Yan, WANG Tongmin, LI Tingju
图2 采用不同平均粒径HEA颗粒改性的Al12Si-HEA试样的力学性能
Fig.2 Engineering stress-strain curves (a) and tensile properties (b) of Al12Si-HEA samples modified with different average size HEA particles