金属塑性成形的应变路径效应:机制、表征与应用
|
樊晓光 1,2,3, 肖云腾 1,2, 詹梅 1,2(  ), 马飞 1,2, 高鹏飞 1,2, 郑泽邦 1,2, 张昕 2,3, 邵光大 2,4, 伍寓铭 1,2
|
|
Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
|
FAN Xiaoguang 1,2,3, XIAO Yunteng 1,2, ZHAN Mei 1,2(  ), MA Fei 1,2, GAO Pengfei 1,2, ZHENG Zebang 1,2, ZHANG Xin 2,3, SHAO Guangda 2,4, WU Yuming 1,2
|
|
|
图15. 标准等通道转角挤压(ECAP)路线下的变形应变路径[116]
|
Fig.15. Deformation strain paths under standard equal channel angular pressing (ECAP) routes[116] (a) illustration of a cubic element undergoing defor-mation due to shearing after a single pass of ECAP (b) evolution of deformation in each plane for all 4 ECAP routes after up to 8 passes of ECAP
|
|
 |
|
|