Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
|
|
图14. 不同应变路径下制备的Al/Mg复合板材拉伸性能对比[ |
Fig.14. Comparisons of tensile properties of Al/Mg composite sheets fabricated under single pass (sp) and double passes by direct rolling (dpd), reverse rolling (dpr), and cross rolling (dpc)[ |
![]() |