金属塑性成形的应变路径效应:机制、表征与应用
|
|
Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
|
|
图13. 不同加载路径下的α相形态及晶体取向特征[ |
Fig.13. Characteristics of morphology and crystallographic orientation of α phase deformed along different loading paths[ |
![]() |