[an error occurred while processing this directive]
金属塑性成形的应变路径效应:机制、表征与应用
樊晓光1,2,3, 肖云腾1,2, 詹梅1,2(), 马飞1,2, 高鹏飞1,2, 郑泽邦1,2, 张昕2,3, 邵光大2,4, 伍寓铭1,2
Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
FAN Xiaoguang1,2,3, XIAO Yunteng1,2, ZHAN Mei1,2(), MA Fei1,2, GAO Pengfei1,2, ZHENG Zebang1,2, ZHANG Xin2,3, SHAO Guangda2,4, WU Yuming1,2

图6. AZ31镁合金在不同应变路径约束槽挤压(CGP)过程中的应变累积示意图[40]

Fig.6. Schematics of strain accumulation of AZ31 magnesium alloy during constrained groove pressing(CGP)[40] (TD—transverse direction)
(a) one pass of CGP and two passes of 180° cross-CGP (b) two passes of 90° cross-CGP