金属塑性成形的应变路径效应:机制、表征与应用
|
樊晓光 1,2,3, 肖云腾 1,2, 詹梅 1,2(  ), 马飞 1,2, 高鹏飞 1,2, 郑泽邦 1,2, 张昕 2,3, 邵光大 2,4, 伍寓铭 1,2
|
|
Strain Path Effects in Metal Plastic Forming: Mechanisms, Characterization, and Application
|
FAN Xiaoguang 1,2,3, XIAO Yunteng 1,2, ZHAN Mei 1,2(  ), MA Fei 1,2, GAO Pengfei 1,2, ZHENG Zebang 1,2, ZHANG Xin 2,3, SHAO Guangda 2,4, WU Yuming 1,2
|
|
|
图3. QP980钢在不同预应变条件下的应力-应变曲线[29]
|
Fig.3. Stress-strain curves of quenching and partitioning steel (QP980) specimens at various pre-strain levels deformed along RD[29] (UT-UC—uniaxial tension (UT) followed by compression,UC-UT—uniaxial compression (UC) followed by tension, RD—rolling direction, T—tension, C—compression) (a) UT-UC (b) UC-UT
|
|
 |
|
|