热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图9. 锌镀层对热成形钢氢脆风险的影响[8,85]

Fig.9. Influences of Zn coating on the hydrogen embrittlement risk of PHS[8,85] (a, b) tensile curves (a) and thermal desorption analysis (TDA) curves (b) of aluminized, uncoated, and galvanized PHS austenitized at 900  oC for an aus-tenitizing time (tA) of 6 min[8] (c) evolution of localized necking elongation (elon-gation from ultimate tensile strength up to fracture) with strain rate for a Zn-coated steel in 3%NaCl solution and air conditions[85]