热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图8. 夹杂物对氢脆的影响[71,74]

Fig.8. Influences of inclusions on hydrogen embrittlement (a-c) high-resolution tritium autoradiographies of FeS (a), TiN (b), and MnS (c), respectively, as hydrogen traps[71.74] (d) fisheye morphology on the fracture surface of PHS1900 after hydrogen charging[71] (e) enlarged image of Fig.8d[71] (e1-e5) EDS analyses of the inclusion in Fig.8e[71]