[an error occurred while processing this directive]
热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图7. NbC对高强度马氏体钢抗氢脆性能的影响[63]

Fig.7. Influences of NbC on hydrogen embrittlement resistance of high-strength martensitic steels[63] (a-c) tensile stress-strain curves with and without hydrogen charging for martensitic steels as-quenched (900-Q') (a), tempered at 480 oC (Q&T-480) (b), and tempered at 560 oC (Q&T-560) (c) (HC—hydrogen pre-charged) (d) thermal desorption spectroscopy (TDS) curves (The TDS profiles corresponding to the temperature range from 300 oC to 500 oC are shown in the enlarged inset) (e) schematics showing how NbC nano-precipitates enhance hydrogen embrittlement resistance