[an error occurred while processing this directive]
热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图6. 组织细化对1800 MPa热成形钢微观组织和抗氢脆性能的影响[61]

Fig.6. Influences of grain refinement on the microstructure and hydrogen embrittlement resistance of 1800 MPa PHS[61] (a, b) SEM image (a) and EBSD IPF (b) of Nb free steel (c, d) SEM image (c) and EBSD IPF (d) of Nb steel (e) plots of fracture stress vs H concentrations of the Nb and Nb free steels acquired using the notch tensile samples (Error bars of the fracture stress represent the standard deviation of three pre-charge tensile tests for the same charging time)