[an error occurred while processing this directive]
热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图5. 拉伸强度为1500和2000 MPa的热成形钢的断裂韧性和裂纹扩展行为[47]

Fig.5. Fracture toughnesses and crack propagation behaviors of press hardening steel (PHS) with tensile strengths of 1500 and 2000 MPa[47]
(a) J-integral-based resistance curves (J-R curves) measured from the side-grooved compact tension specimens at room temperature
(b) corresponding fracture toughness in terms of K (K is the mode I stress intensity factor, which characterizes the elastic stress field at the crack tip and reflects the fracture resistance of materials. KJIc and KJss represent crack-initiation toughness and crack growth toughness in terms of K, respectively)
(c) complete stress-displacement curves of PHS notched samples under long charging durations
(d) magnified regions in Fig.5c after the respective peak stress