[an error occurred while processing this directive]
热成形汽车钢的弯曲韧性与氢脆行为研究进展
杜德灏1,2,3, 管明1,2, 曹祚恒1,2, 王铭1,2(), 何斌斌3, 黄明欣1,2()
A Review of Current State and Prospects of the Bendability and Hydrogen Embrittlement Behavior of Press- Hardening Automobile Steels
DU Dehao1,2,3, GUAN Ming1,2, CAO Zuoheng1,2, WANG Ming1,2(), HE Binbin3, HUANG Mingxin1,2()

图1. 热冲压前后Al-Si镀层硼钢横截面分层结构的SEM像[5]

Fig.1. Cross-sectional SEM images of the Al-Si coated boron steel before (a, b) and after (c) press hardening[5]
(a) as-coated (b) detail of intermetallic layer (c) austenitized at 920 oC for 5 min