原位反应粉末冶金铝基复合材料界面研究进展
|
|
赵乃勤, 王振博, 戎旭东, 赵冬冬, 何春年
|
Advances in Interface of Powder Metallurgy Aluminum Matrix Composites Fabricated via In Situ Reaction: A Review
|
|
ZHAO Naiqin, WANG Zhenbo, RONG Xudong, ZHAO Dongdong, HE Chunnian
|
|
表1 原位反应粉末冶金铝基复合材料中涉及的主要原位反应体系、制备方法、特点及其应用领域[34,35,40,43,54,55,59,60,64~66]
|
Table 1 Main in situ reaction system, preparation methods, characteristics, and application fields involved in powder metallurgy Al matrix composites (AMCs) fabricated via in situ reaction[34,35,40,43,54,55,59,60,64-66]
|
|
| System | Preparation method | Advantage | Disadvantage | Application field |
|---|
| Ex situ carbon materials/Al[34,35] | Ball milling + sintering | Simple process | Difficulty in dispersion control, interface reactions not easily regulated | High-strength conductive components, electronic packaging, precision instruments | | In situ synthesized carbon materials/Al[40,43] | In situ growth by CVD | Uniform reinforcement distribution, good interface bonding | Complex process, high cost, limited production | | Oxide/Al[54,55] | Sintering reaction | High reaction driving force, good thermal stability of reinforcements | Difficult to control precursor ratio and reaction kinetics | Lightweight structural components, wear-resistant parts, heat-resistant alloy substitutes | am-Al2O3/Al[59,60] | Ball milling pre-treatment + sintering reaction | Good thermal stability and high-temperature performance | Possible crystallization of amorphous phase at high temperatures | | Al-Ti-X (X = C, B, Si)[64-66] | Sintering reaction | High hardness and good thermal stability of reinforcements | Complex reaction pathways in multi-component systems |
|
|
|