[an error occurred while processing this directive]
原位反应粉末冶金铝基复合材料界面研究进展
赵乃勤(), 王振博, 戎旭东, 赵冬冬, 何春年
Advances in Interface of Powder Metallurgy Aluminum Matrix Composites Fabricated via In Situ Reaction: A Review
ZHAO Naiqin(), WANG Zhenbo, RONG Xudong, ZHAO Dongdong, HE Chunnian

图6. 基于界面修饰策略制备铝基复合材料的微观组织[90,91]

Fig.6. Microstructures of AMCs fabricated by interface decoration strategy
(a-f) STEM image of GNPs-Cu nanoplatelets (NPLs) (a), HRTEM image of GNPs-Cu hybrid structure (b), STEM image of GNPs-Cu/Al composite powders (c), and HRTEM image and corresponding FFT and IFFT of the marked box region at the interface between GNPs-Cu NPL and Al matrix (d-f)[90] (BF—bright field)
(g, h) TEM images of as-synthesized Cu2O@CNTs powders (Inset in Fig.6g is the related image of Cu2O@CNTs powders dispersed in ethanol; insets in Fig.6h are corresponding EDS mapping and FFT image)[91]
(i) typical HAADF-STEM image of the Cu2O@CNTs/Al composite (Inset shows the O element distribution)[91]
(j-l) TEM image of CNTs-Al interface (j) and magnified images of the frames I (k) and II (l) recorded in Fig.6j (Inset in Fig.6l shows the statistical result of the diameter of CuAl2 precipitates (indicated by white arrows in Fig.6j))[91]