[an error occurred while processing this directive]
原位反应粉末冶金铝基复合材料界面研究进展
赵乃勤(), 王振博, 戎旭东, 赵冬冬, 何春年
Advances in Interface of Powder Metallurgy Aluminum Matrix Composites Fabricated via In Situ Reaction: A Review
ZHAO Naiqin(), WANG Zhenbo, RONG Xudong, ZHAO Dongdong, HE Chunnian

图5. 基于固相扩散策略制备原位反应铝基复合材料界面的TEM像[54,77]

Fig.5. TEM images of the interfaces of in situ reaction AMCs fabricated by solid-phase diffusion strategy
(a-f) HRTEM images of MgAl2O4 interface (a-d) and MgAlB4/Al interface (e, f)[77]
(g) HRTEM image of the Al2O3/Al interface with corresponding FFT (inset)[54]
(h) stereographic projection on (22¯0) plane, [112] zone axis of Al (marked by red) and (311) plane, [01¯1] zone axis of Al2O3 (marked by yellow)[54]
(i) “Al2O3-intermixing region-Al” interface structure with corresponding FFT and inverse FFT (IFFT)[54]