[an error occurred while processing this directive]
原位反应粉末冶金铝基复合材料界面研究进展
赵乃勤(), 王振博, 戎旭东, 赵冬冬, 何春年
Advances in Interface of Powder Metallurgy Aluminum Matrix Composites Fabricated via In Situ Reaction: A Review
ZHAO Naiqin(), WANG Zhenbo, RONG Xudong, ZHAO Dongdong, HE Chunnian

图3. CuO/Al复合材料、B2O3/Al复合材料和TiO2/Al复合材料的微观组织[55~58]

Fig.3. Microstructures of CuO/Al composite, B2O3/Al composite, and TiO2/Al composite (a, b) distributions of Al2O3 (a) and Al-Cu intermetallic compounds formed in CuO/Al composite (b)[55] (c-h) TEM (c, e, g) and HRTEM (d, f, h) images of secondary phases in the CuO/Al composite[56] (Insets in Figs.3d-f are corresponding fast Fourier transform (FFT)) (i, j) SEM images showing the distributions of Al2O3 and AlB2 in the B2O3/Al composites with different magnificaitons[57] (k-n) TEM images of Al3Ti (k, l), Al-Al3Ti interface (m), and Al2O3 (n) in the TiO2/Al composite[58] (Insets in Figs.3k and n are corresponding SAED patterns)