[an error occurred while processing this directive]
原位反应粉末冶金铝基复合材料界面研究进展
赵乃勤(), 王振博, 戎旭东, 赵冬冬, 何春年
Advances in Interface of Powder Metallurgy Aluminum Matrix Composites Fabricated via In Situ Reaction: A Review
ZHAO Naiqin(), WANG Zhenbo, RONG Xudong, ZHAO Dongdong, HE Chunnian

图2. 通过化学气相沉积(CVD)技术原位合成CNT/Al复合材料和石墨烯纳米片(GNPs)/Al复合材料的制备过程示意图及微观组织[40,43]

Fig.2. Preparation process schematics and microstructures of the in situ synthesized CNT/Al composites and graphene nanosheets (GNPs)/Al composites by chemical vapor deposition (CVD) technology
(a) preparation process schematic of CNT/Al composites[40]
(b, c) TEM images of in situ synthesized CNTs (b) and CNT/Al composite (c)[40] (Inset in Fig.2b shows the magnified image of CNT)
(d) preparation process schematic of GNPs/Al composites[43]
(e, f) TEM images of in situ synthesized GNPs/Al composite powders (e) and CNT/Al composite (f)[43] (Inset in Fig.2e is the SAED pattern of the red solid box; and inset in Fig.2f is the SAED pattern of the blue solid box)