基于同步辐射原位表征技术的镁合金研究进展
郭恩宇1,2(), 杜泽龙1, 李炳志1, 王同敏1,2()
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
GUO Enyu1,2(), DU Zelong1, LI Bingzhi1, WANG Tongmin1,2()

图6. 同步辐射成像技术在镁合金腐蚀防护领域的应用[81,82,85,86]

Fig.6. Applications of synchrotron imaging technology in the corrosion protection of magnesium alloys
(a) 3D reconstructed images before and after 360 h immersion in 3.5%NaCl (mass fraction) solution for LAZWMVT alloy (Mg-Li-Al-Zn-Y-Mn-Gd-Sn alloy) under in situ corrosion observation, with secondary phase distributions indicated (Green represents Alₓ(Gd, Y, Mn) phase, red denotes Mg2Sn phase, light blue marks AlLi phase, and yellow highlights corrosion pits)[81]
(b) time-dependent corrosion morphologies of Mg-Sn alloy in NaCl solution monitored via in situ corrosion observation, and schematic diagram and physical device of in situ corrosion imaging experiment at SSRF[82]
(c) 3D reconstructions of the interface between MAO-SSC coating on LA81 Mg-Li alloy surface obtained through in situ corrosion observation[85] (MAO—micro-arc oxidation, SSC—solid-like slippery composite coating)
(d) 3D reconstructions of simulated ZX50 and MAO implant sites showing visible bubble structures (in light blue) via in situ corrosion observation[86]