[an error occurred while processing this directive]
基于同步辐射原位表征技术的镁合金研究进展
郭恩宇1,2(), 杜泽龙1, 李炳志1, 王同敏1,2()
Research Progress on Magnesium Alloys Based on Synchrotron Radiation In Situ Characterization Techniques
GUO Enyu1,2(), DU Zelong1, LI Bingzhi1, WANG Tongmin1,2()

图5. 同步辐射X射线原位成像技术在镁合金损伤断裂过程中的典型应用[67,70,71]

Fig.5. Typical applications of synchrotron radiation X-ray in situ imaging technology in the damage and fracture process of magnesium alloys
(a) von Mises stress (S) distributions on the particles in composites with various particle sizes at 0.8% strain and the fracture process of a representative particle[67] (ε—true strain. The stress concentration was indicated by red arrows)
(b, c) 2D slices (b) and 3D (c) fracture morphologies of composites[67] (White arrows in Fig.5b indicate microcracks. The blue regions in Fig.5c represent the microcracks)
(d) void/microcrack link-up via micro-scale localization in the surface-scans of the sample[70] (The three principal directions are labeled as longitudinal (L), which corresponds to the rolling direction, transverse (T) and short-transverse (S) through the thickness)
(e) reconstructed X-ray images showing cracks near the surface of the sample[71] (F—force. The arrow in the bottom left image of Fig.5e shows a shear-like linkage between cracks, while the arrow in bottom right image shows a deflected fatigue crack propagation path)